Purifying?agent?for?molten?zinc?in?HDG
Name:
Purifying?agent?for?molten?zinc?in?HDG
  • Model:
  • Uses:
  •  
Details

In the light of the high iron and impurity contents in molten zinc, poor fluidness and particles and fold on workpiece often occurred in hot galvanizing plants, our company has organized the famous specialists and scientific and technological personnel in many disciplines at home developed XY-XG-3 type purifying agent for molten zinc, a high and new technical product. It has effectively solved the difficult problem and filled in the gap in this field at home. Through testing and using, the agent reached the anticipated results and is well received by customers. At present the product is applying for a patent. 
Notice
Do well pretreatment work, do not carry the harmful impurity into zinc pot, galvanizing agent needs the acid and iron eliminating, and it would be best if rinsing water for pretreatment could be fluid.
Because of the high volatility of the agent, No.2 operation should be quickly performed.
In order to avoid the splashing of molten zinc causing danger, operators should be well dressed in labor protection articles. Operation with caution and safety first.
Purifying Treatment Method of Molten Zinc:
Keep furnace temperature at 450℃-470℃.
Place dry thermal insulation bricks (with strong water absorption) into box with holes, quickly pour the purifying agent to them, insert the box into molten zinc and move it back and forth until boiling ends, and take out the box with holes.
Eliminate suspended substances on the surface of molten zinc; scatter ammonium chloride (1-1.5 kg/ m2) to further eliminate impurity on the surface.
Repeat the abovementioned steps three or four times.
Add the alloy, which is 0.5% of molten zinc, in uniform distribution way. After all the melting, repeat the abovementioned step once. (If there are excessive aluminum or other alloys in original molten zinc, the step-by-step method can be used)
The temperature is controlled at 430℃-440℃ and the standing time is 6-12 h (time is as long as possible).
When small workpiece is tested (the temperature is at 430℃ and dipping time is not changed), the surface and coating thickness is measured. If the coating is thick, the alloy, which is 0.1 % of molten zinc, can be added. 
The zinc and the alloy can be added at one time until the alloy content in molten zinc reaches 1.5%.
After alloying is completed, the working temperature of molten zinc should be controlled at 440℃±5℃ and the lifting speed of traveling crane at 1.5 m / min.
 

 

返回頂部 電話
主站蜘蛛池模板: 成年网站免费观看| 99re在线播放| 大开眼界 无删减| 草草影院浮力| 欧美一级www片免费观看| 自拍 第一页| 日本黄色大片免费看| 无码av片av片av无码| 精品久| 后入内射无码人妻一区| 黄色a视频| a毛看片免费观看视频| 丝袜偷窥亚洲综合| 亚洲伊人精品| 午夜dj在线观看免费视频| 久草在线视频在线| 国内精品人妻无码久久久影院导航| 欧美xxxx狂喷水喷水| 99精品国产成人一区二区| 亚洲人成无码www久久久| 精品推荐国产麻豆剧传媒| 欧美性猛交xxxx乱大交极品| 日本人视频jizz69页码| 九色网址| 亚洲熟妇无码av另类vr影视| 亚洲欧美日韩中文综合v日本| 九九久久精品无码专区| 日本在线播放一区二区| 亚洲精品第一国产综合高清| 欧美最猛黑人xxxx黑人猛交| 国产电影一区二区| 免费一二区| 无码粉嫩虎白一线天在线观看| 久久中文视频| 欧美性video| 久久精品水蜜桃av综合天堂| 韩国A片国产浪潮AV| 婷婷在线五月| 国内精品久久久久久久影视麻豆 | 337p日本欧洲亚洲大胆| 永久黄网站免费视频性色|